TEMPERATURA TOPNIENIA (℃) | GĘSTOŚĆ (g/cm3) | LEPKOŚĆ (mpa.s 140°C) | OPAKOWANIA ( KG ) | JAK UŻYWAĆ |
110 | 0,95-0,97 | 9-25 | 25 (TORBA MIESZANA) | MOŻNA JĄ DODAWAĆ W KAŻDYM KROKU.WTEDY NALEŻY BYĆ JEDNORODNO ROZPROWADZONY. |
JEST TO WOSK FISCHER TROPSCH O DOBREJ POZIOMIE I ODPORNOŚCI NA ZARYSOWANIA.NIE BĘDZIE PRODUKOWAĆ DYMU.JEST BARDZO ZALECANY PRZY APLIKACJI MATÓW PROSZKOWYCH.
ZALECANA ILOŚĆ DODATKU TO 0,5-1,5% CAŁKOWITEJ ILOŚCI FORMUŁY.MOŻESZ WYBRAĆ OPTYMALNĄ ILOŚĆ WEDŁUG RÓŻNYCH POTRZEB PRAKTYCZNYCH.
TEMPERATURA TOPNIENIA (℃) | STOPIEŃ PENETRACJA (10-1mm) | ŚREDNIA WIELKOŚĆ CZĄSTEK (μm) | OPAKOWANIA ( KG ) | JAK UŻYWAĆ |
120 | <1,0 | 4-6 | 20 (TORBA MIESZANA) | MOŻNA JĄ DODAWAĆ W KAŻDYM KROKU.WTEDY NALEŻY BYĆ JEDNORODNO ROZPROWADZONY. |
JEST TO RODZAJ MIKRONIZOWANEGO WOSKU FISCHER TROPSCH O RÓWNOMIERNIE ROZŁOŻONEJ MAsie MOLEULNEJ.MA NIEWIELKI WPŁYW NA POŁYSK I DOBRĄ ROZPROSZALNOŚĆ.ZALECANY DO STOSOWANIA FARB PRZEMYSŁOWYCH, WOSKÓW DO POWŁOK PROSZKOWYCH ORAZ FARB DRUKARSKICH OFFSETOWYCH.JEST BARDZO EKONOMICZNY.
ZALECANA ILOŚĆ DODATKU WYNOSI 0,5~1,0% CAŁKOWITEJ ILOŚCI FORMUŁY.PROSZĘ WYBRAĆ OPTYMALNĄ ILOŚĆ WEDŁUG RÓŻNYCH POTRZEB PRAKTYCZNYCH.
TEMPERATURA ZAMRAŻANIA °C | TREŚĆ % | ODCZYN JODOWY | OPAKOWANIA ( KG ) |
60,0-70,0 | ≥90% | gI2/100g≦4,0 | 25(TORBA ZŁOŻONA) |
Jest to rodzaj nietoksycznego plastyfikatora, środka przeciwstarzeniowego i środka spieniającego, szeroko stosowanego do produkcji keratonu w proszku.SKUTECZNIE POPRAWIA ELASTYCZNOŚĆ, PLASTYCZNOŚĆ I WŁAŚCIWOŚCI ANTYSTATYCZNE PRODUKTU.
JEST TO RODZAJ BIAŁEGO PROSZKU ZASADNICZO WOLNY OD ZANIECZYSZCZEŃ. JEST NIEROZPUSZCZALNY W WODZIE ORAZ ROZPUSZCZALNY W ALKOHOLU, benzenie i acetonie.PODCZAS INTENSYWNEGO WSTRZĄŚNIĘCIA Z GORĄCĄ WODĄ BĘDZIE Emulgować do stałej, wodorozcieńczalnej dyspersji polimerowej.WARTOŚĆ HLB ZAWIERAJĄCA 90% MONOSTEARYNY WYNOSI 3,9-5,3.JEST TO RODZAJ Emulgatora WIELOZADANIOWEGO, KTÓRY JEST BEZPIECZNYM, UZNANYM W MIĘDZYNARODZIE DODATKEM DO ŻYWNOŚCI BEZ OGRANICZONEJ ILOŚCI ZASTOSOWANIA PRZEZ FDA.
TEMPERATURA Zeszklenia °C | WARTOŚĆ KWASOWA(mg/gKOH) | WYGLĄD | OPAKOWANIA ( KG ) |
125 | 285 | CZĄSTECZKI LUB PROSZEK | 25 |
JEST TO TYP REAKCJI ŚRODKA MATUJĄCEGO DO POWŁOK PROSZKOWYCH.DOTYCZY TRANSPARENTNYCH I MATOWYCH POWŁOK PROSZKOWYCH.
JEST MATOWY CZARNY BEZ WYBIELAŃ.POSIADA DOBRĄ ODPORNOŚĆ NA ZARYSOWANIA.
TEMPERATURA TOPNIENIA (℃) | WARTOŚĆ KWASOWA (mg/gKOH) | LICZBA AMIN (mg/gKOH) | OPAKOWANIA ( KG ) |
141,5-146,5 | ≤7,5 | ≤2,5 | 25 |
STOSOWANY JEST W POSTĘPIE ODPIANIAJĄCYM PRZY STOSOWANIU POWŁOK PROSZKOWYCH, ŻELIWA I ALUMINIUM.
ILOŚĆ DODATKU ZMIENIA SIĘ W ZALEŻNOŚCI OD ILOŚCI WYPEŁNIACZY PIGMENTOWYCH.DODATKOWA ILOŚĆ ŚRODKA ODPIENIAJĄCEGO: 0,5 ~ 5% ILOŚCI WYPEŁNIACZA.
KATEGORIA PRODUKTU | TEMPERATURA TOPNIENIA (℃) | WARTOŚĆ KWASOWA (mg/gKOH) | WYGLĄD | OPAKOWANIA ( KG ) |
PRZECIWUTLENIACZE | 160-180°C | ≤1,0 | PROSZEK O LEKKIM ZAPACHU | 25 |
ZWYKLE NIE JEST UŻYWANE ODDZIELNIE.JEST SZERoko stosowany w zastosowaniach materiałów makrocząsteczkowych, takich jak PE, PP, PS, POLIAMID, POLIWĘGLAN I ABS, PO Zmieszaniu Z PRZECIWUTLENIACZAMI FENOLOWYMI.
JEST TO RODZAJ ORGANICZNEGO ESTRU FOSFRYNOWEGO O WYSOKICH WYDAJNOŚCIACH.POMAGA ZAPOBIEGAĆ PRZEBARWIENIOM POLIMERÓW.SZYBKOŚĆ DEGRADACJI POLIMERÓW MOŻE BYĆ OBNIŻONA.MOŻNA POPRAWIĆ ODPORNOŚĆ ŻYWICY NA PADANIE GAZU.
KATEGORIA PRODUKTU | TEMPERATURA TOPNIENIA (℃) | WIELKOŚĆ CZĄSTEK (μm) | WYGLĄD | OPAKOWANIA ( KG ) |
ŚRODKI PRZECIWZARYSOWANIOWE | 320°C | D50:4,D99:10 | BIAŁY PROSZEK | 25 |
Dzięki niemu papier z folii aluminiowej jest łatwy do rozdrabniania.
JEST TO CZYSTY WOSK PTFE, KTÓRY ZNACZNIE POPRAWIA WŁAŚCIWOŚCI PRZECIWZARYSOWANIOWE, ODPORNOŚĆ NA ŚCIERANIE ORAZ GŁADKOŚĆ POWŁOKI.